Astrid Falkner (BA): Influence of minor elements on the crack susceptibility of nickel-based superalloys – Characterization using the SEBR method
Date: 17. November 2025Time: 13:00 – 13:30Location: WTM Seminar-Room (223) & Zoom
Title: Influence of minor elements on the crack susceptibility of nickel-based superalloys - Characterization using the SEBR method
Advisor: Julius Weidinger
https://fau.zoom-x.de/j/64796390981?pwd=R0hJM1F6aThLZys1MS9CWmk1Uk9RUT09
Meeting-ID: 647 9639 0981
Kenncode: 116776
Event Details
WTM Seminar-Room (223) & Zoom